Mortar is classified by compressive strength using the letters M, S, N, O, and K in descending order of strength. The acronym "MaSoN wOrK" helps remember the order. Standard mortar is a mixture of Portland cement, hydrated lime, and sand. Pre-blended mortars (Type N or Type S) are widely available and ensure consistent proportions.
| Type | Min PSI (28-day) | Cement:Lime Ratio (by volume) | Portland parts | Lime parts | Sand parts |
|---|---|---|---|---|---|
| M | 2,500 PSI | 1:0.25 | 1 | 1/4 | 2.25 — 3 |
| S | 1,800 PSI | 1:0.25 — 1:0.5 | 1 | 1/4 — 1/2 | 2.25 — 3 |
| N | 750 PSI | 1:0.5 — 1:1.25 | 1 | 1/2 — 1-1/4 | 2.25 — 3 |
| O | 350 PSI | 1:1.25 — 1:2.5 | 1 | 1-1/4 — 2-1/2 | 2.25 — 3 |
| K | 75 PSI | 1:2.5 — 1:4 | 1 | 2-1/2 — 4 | 2.25 — 3 |
| Type | Best For | Do NOT Use For |
|---|---|---|
| M | Below-grade foundations, retaining walls, heavy loads, high seismic zones | Above-grade walls where flexibility is needed |
| S | Structural walls, exterior veneer, high wind zones, patios, walks | Historic restoration (too strong) |
| N | General purpose. Above-grade walls, interior/exterior, chimneys, brick veneer | Below-grade or retaining walls |
| O | Interior non-load-bearing, historic restoration (soft brick), repointing soft masonry | Exterior structural, any load-bearing wall |
| K | Historic preservation only. Extremely soft. Interior restoration of historic structures | Any modern structural application |